SNOW-WHITE CERAMIC GYPSUM

Product description

SNOW-WHITE CERAMIC GYPSUM is designed for production of gypsum tiles, panels, mouldings and accessories as well as industrial production of ceramic forms.

Main properties

  • Pot life: approx. 10 minutes
  • Beginning of setting: after approx. 8 minutes

Main parameters

    USE

    Go top
    SNOW-WHITE CERAMIC GYPSUM is designed for production of gypsum tiles, panels, mouldings and accessories as well as industrial production of ceramic forms. Can also be used for preparation of gypsum mortars (top finishes, filling compounds), possibly for repairs of wall and ceiling surfaces (e.g. filling gaps, masking screw holes, etc.), assembly and installation works (mounting electrical boxes, filling furrows). Gypsum mortars and prefabricated elements can only be used indoors.

    PROPERTIES

    Go top
    SNOW-WHITE CERAMIC GYPSUM is a gypsum binder sourced from the process of partial dehydration and milling of natural gypsum stone. Characterised by very fine aggregate, high strength and snow-white colour. It is ecological, fast-setting, convenient and easy in use.

    MORTAR PREPARATION

    Go top
    Pour the dry mix into a container with appropriate amount of clean water (recommended ratio: approx. 0.8 l of water for 1 kg of gypsum), mix manually or mechanically until homogenous and free of lumps. The mass consistency should be adjusted to individual production task or type of use. The mass can be used directly after mixing and keeps plasticity for approx. 10 minutes. Before the next batch mixing, clean the container of residues of set mortar, as it can shorten the time of setting of the next mix.

    APPLICATION

    Go top
    Depending on use.

    CONSUMPTION

    Go top
    Depending on use.

    PACKAGES

    Go top
    Paper bags 20 kg.
    Pallet: 1080 kg in 20 kg bags.

    STORAGE AND TRANSPORT

    Go top
    Shelf life is 6 months from the production date given on the bag. Transport and store the product in tightly closed bags, on pallets, in dry conditions. Protect against humidity. Incoherence with recommendations listed above may impact the product working parameters.

    TECHNICAL DATA

    Go top
    Mixing ratio:
    ca. 0.8 l of water for 1 kg of dry mix
    ca. 16.0 l of water for 20 kg of dry mix
    Content of calcium sulphate (CaSO4)
    >50%
    Pot life:
    approx. 10 minutes
    Beginning of setting:
    after approx. 8 minutes
    Substrate and ambient temperature:
     
    from +5 °C to +25 °C
    Compressive strength:
    ≥ 4.0 N/mm²
    Flexural strength:
    ≥ 2.0 N/mm²
     
    Standard marking
    Gypsum binder for direct use or further processing, for indoor use.
    EN 13279-1-A1
    Reaction to fire
    Class A1
    Airborne sound insulation
    NPD
    Thermal resistance
    NPD
     
    Conforms to the requirements of PN-EN 13279-1:2009 standard.
    Declaration of Performance no. D171/CPR.
    The product has been given the radiation hygiene certificate.
     
    NOTE
    Keep out of the reach of children. Do not breathe dust. Avoid contact with skin and eyes. In case of contact with eyes, rinse immediately with plenty of water and seek medical advice. Do not empty into drains. Wear suitable protective clothing and eye/face protection. If swallowed, seek medical advice immediately and show this container or label.
     